欢迎访问《中外公路》官方网站,今天是
分享到:
基于弯沉响应的路面结构性裂缝评价指标研究
CSTR:
作者:
作者单位:

1.江苏交通控股有限公司,江苏 南京 210005;2.江苏高速公路工程养护技术有限公司,江苏 南京 211100;3.河海大学 土木与交通学院,江苏 南京 210024;4.江苏宁宿徐高速公路有限公司,江苏 宿迁 223800;5.江苏沿江高速公路有限公司,江苏 苏州 215000

作者简介:

郑俊秋,男,硕士,工程师.E-mail:447832674@qq.com

通讯作者:

朱浩然,男,博士,副教授.E-mail:dndxzhr@qq.com

中图分类号:

U416.2

基金项目:

国家自然科学基金资助项目(编号:52378448); 江苏交控重大专项(编号:2021JKY01)


Evaluation Index of Pavement Structural Cracks Based on Deflection Response
Author:
Affiliation:

1.Jiangsu Communications Holding Co., Ltd., Nanjing, Jiangsu 210005, China;2.Jiangsu Expressway Engineering Maintenance Technology Co., Ltd., Nanjing, Jiangsu 211100, China;3.College of Civil and Transportation Engineering, Hohai University, Nanjing, Jiangsu 210024, China;4.Jiangsu Ningsuxu Expressway Co., Ltd., Suqian, Jiangsu 223800;5.Jiangsu Yanjiang Expressway Co., Ltd., Suzhou, Jiangsu 215000, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为准确评估结构性裂缝对路面结构强度的影响并建立相应的评价指标,该文在江苏省多条高速路段开展现场试验。采用落锤式弯沉仪对裂缝左右3 m范围内15个测点进行检测,并绘制各测点处中心弯沉曲线,同时根据曲线特征提出弯沉极差、裂缝单侧最大影响距离和影响面积3项裂缝评价指标。通过在试验裂缝正上方取芯,验证裂缝类型与发展层位,并根据芯样中裂缝的分布形态与开裂状况,将结构性裂缝划分为6种类型。结果表明:所提出的3项指标能有效区分疲劳裂缝与结构性裂缝,弯沉极差与影响面积之间R2为0.75,Pearson相关系数为0.88,两者与裂缝发展的各阶段均具有良好对应关系,可协同评估裂缝的严重程度,对路面养护施工具有实际指导价值。

    Abstract:

    To accurately assess the impact of structural cracks on the strength of pavement structures and establish corresponding evaluation indicators based on deflection response, field tests were conducted on multiple sections of expressways in Jiangsu Province. A falling weight deflectometer was used to test a total of 15 measurement points within a 3-meter range on both sides of each crack. The center deflection values at each measurement point were plotted into curves, and three evaluation indicators for cracks, namely deflection range, maximum influence distance on one side of the crack, and influence area, were proposed based on the characteristics of the curves. Core samples were taken directly above the selected cracks within the test sections to verify the crack types and development layers. According to the distribution and cracking conditions of the cracks in the core samples, six types of structural cracks were classified. The results show that the proposed indicators can effectively distinguish fatigue cracks from structural cracks. The coefficient of determination (R2) between deflection range and influence area is 0.75, and the Pearson correlation coefficient is 0.88. Both indicators have a good correspondence with the various stages of crack development and can be used in combination to evaluate the severity of cracks, providing practical guidance for pavement maintenance and construction.

    参考文献
    相似文献
    引证文献
引用本文

郑俊秋,马辉,乔月来,等.基于弯沉响应的路面结构性裂缝评价指标研究[J].中外公路,2025,45(5):27-34.
ZHENG Junqiu, MA Hui, QIAO Yuelai, et al. Evaluation Index of Pavement Structural Cracks Based on Deflection Response[J]. Journal of China & Foreign Highway,2025,45(5):27-34.

复制
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2025-06-18
  • 最后修改日期:2025-07-25
  • 录用日期:
  • 在线发布日期: 2025-10-27
  • 出版日期:
文章二维码
网站二维码
期刊公众号